26 Apr 2017
Viewed 218 Times 0 Comments

Repairs should be made by cutting out the damaged section and grinding the surrounding area to a roughened, feathered surface extending 100 mm in each direction from the damaged area. The area to be covered should be thoroughly cleaned with a stiff brush. Glass mat and Base Resin should be used to make good the repair, left to harden and subsequently the Topcoat re-applied. Care should be taken not to coat existing areas of Topcoat.

Was this answer helpful ? Yes (0) / No (0)